Brand Name : Wuxi Jinlai
Model Number : Nickle Bar
Certification : ISO
Place of Origin : CHINA
MOQ : 3 tons
Price : negotiable based on the quantity
Payment Terms : T/T, Western Union, L/C
Supply Ability : 6000 tons per month
Delivery Time : 30-60 days
Packaging Details : Standard seaport packing or as custom request
Grade : Nickle
Standard : AISI, ASTM, BS, DIN, GB, JIS
Diameter : 50-75 mm
Ni (Min) : 57%
Ultimate Strength (≥ MPa) : 900
Elongation (≥ %) : 30
Application : Industry
Port : Shanghai
Product Name | High temperature nickel based alloy powder Hastelloy C-22 Inconel 718 Inconel 713C |
Material | Monel/Inconel/Hastelloy/Duplex Steel/PH Steel/Nickel Alloy |
Shape | Round,Forging,Ring,Coil,Flange,Disc,Foil,Spherical,Ribbon,Square,Bar,Pipe,Sheet |
Grade | Alloy:alloy 20/28/31 |
Hastelloy:Hastelloy B/-2/B-3/C22/C-4/S/C276/C-2000/G-35/G-30/X/N/g; | |
Hastelloy B/UNS N10001.hastelloy B-2/UNS N10665/ DIN W.Nr 2.4617,Hastelloy C,HastelloyC-4/UNS N06455/DIN W.Nr,2.4610,HastelloyC-22/UNS N06022/DIN W.Nr.2.4602,Hastelloy X/UNS N0602/DIN W.Nr.2.4665 | |
Haynes:Haynes 230/556/188; | |
Inconel Series: | |
Inconel 600/601/602CA/617/625/713/718/738 | |
Inconel 718/uns n07718/ | |
Incoloy:incoloy 800/800H/800HT/825/925/926 | |
GH:GH2132,GH3030,GH3039,GH3128;GH4180;GH3044 | |
Monel:Monel 400/K50/R405 | |
Nitronic:Nitronic 40/50/60 | |
Nimonic :Nimonic 75/80A/90A/A263 | |
Specification | Wire:0.01-10mm Strip:0.05*5.0-5.0*250mm Bar:dia4-50mm,length 2000-5000mm Pipe |
Product Characteristics | 1.According to the preparation process can be divided into deformation superalloys.casting superalloys and power metallurgy superalloys. 2.According to the strengthening mode,there are solid solution strengthening type,precipitation strengthening type,oxide dispersion strengthening type and fober strengthening type,etc... |
Standard | GB,AISI,ASTM,DIN,EN,SUS,UNS etc. |
Inspection | ISO,SGS,BV AND SO ON. |
Application | High temperature components such as turbing blades,guide vanes ,turbine disks,high pressure compressor disks,machine manufacturing |
Packaging | 1.cases packed in wooden cases 2.paper packaging 3.plastic packing 4.foam packaging Packaging according to customer requirements or products |
Delivery | 7-25 days or according to the products |

If you have any question, please feel free to contact us any time.
|
|
50-75mm Casting Superalloy Nicke Basedl Alloy round bars for Industry Images |